Previous slide
Next slide

Test report of 400D UHMWPE Fiber in 2009

The test sample is 400D/240F UHMWPE fiber in original white color and test by CTTC in 2009 and the tenacity was 35.1cN/dtex. Tested Item Result Standard Linear Density 418.2dtex ISO 2060-1994 Diameter 18.12Nano ISO 137-1975 Breaking Tenacity 35.1cN/dtex ISO 2062-1993 CV of breaking tenacity 6.36% Breaking elongation 3.07% CV of breaking elongation 7.73% *The test results are transferred from below Chinese version. Part view of UHMWPE fiber test report – 400D/240F

Read More »

Test report of 200D UHMWPE Fiber in 2008

The test sample is 200D/60F UHMWPE fiber in original white color and test by CTTC in 2008 and the tenacity was 31.7cN/dtex. Tested Item Result Standard Linear Density 222dtex Breaking Tenacity 31.7cN/dtex ISO 2062-1993 CV of breaking tenacity 6.57% Breaking elongation 3.18% CV of breaking elongation 8.55% *The test results are transferred from below Chinese version. Part view of UHMWPE fiber test report – 200D/60F

Read More »

Test report of 800D UHMWPE Fiber in 2014

The test sample is 800D/480F UHMWPE fiber in original white color and test by CTTC in 2014 and the tenacity was 28.6cN/dtex. Tested Item Result Standard Linear Density 907.3dtex GB/T 19975-2005 Breaking Tenacity 28.6cN/dtex GB/T 19975-2005 CV of breaking tenacity 6.41% GB/T 19975-2005 Breaking elongation 2.94% GB/T 19975-2005 CV of breaking elongation 9.34% GB/T 19975-2005 Initial Modulus 1297cN/dtex GB/T 19975-2005 *The test results are transferred from below Chinese version. Part view of UHMWPE fiber test report – 800D/480F

Read More »

Test report of 800D UHMWPE Fiber in 2018

The test sample is 800D/480F UHMWPE fiber in original white color and test by CTTC in 2018 and the tenacity was 35.5cN/dtex. Tested Item Result Standard Linear Density 955.9dtex GB/T 19975-2005 Breaking Tenacity 35.5cN/dtex GB/T 19975-2005 CV of breaking tenacity 7.76% GB/T 19975-2005 Breaking elongation 3.00% GB/T 19975-2005 CV of breaking elongation 8.72% GB/T 19975-2005 Initial Modulus 1620cN/dtex GB/T 19975-2005 *The test results are transferred from below Chinese version. Part view of UHMWPE fiber test report – 800D/480F

Read More »

Test report of 800D UHMWPE Fiber in 2019

The test sample is 800D/480F UHMWPE fiber in original white color and test by CTTC in 2019 and the tenacity was 36.7cN/dtex. Tested Item Result Standard Linear Density 891.6dtex GB/T 19975-2005 Breaking Tenacity 36.7cN/dtex GB/T 19975-2005 CV of breaking tenacity 5.46% GB/T 19975-2005 Breaking elongation 3.25% GB/T 19975-2005 CV of breaking elongation 5.84% GB/T 19975-2005 Initial Modulus 1490cN/dtex GB/T 19975-2005 Oil Content 0.05% GB/T 6504-2008 *The test results are transferred from below Chinese version. Part view of UHMWPE fiber test report – 800D/480F

Read More »

Test report of 1600D UHMWPE Fiber in 2008

The test sample is 1600D/480F UHMWPE fiber in original white color and test by CTTC in 2008 and the tenacity was 27.7cN/dtex. Tested Item Result Standard Breaking Tenacity 27.7cN/dtex ISO 2062-1993 CV of breaking tenacity 5.30% Breaking elongation 2.40% CV of breaking elongation 8.52% *The test results are transferred from below Chinese version. Part view of UHMWPE fiber test report – 1600D/480F

Read More »

Test report of 1600D UHMWPE Fiber in 2014

The test sample is 1600D/960F UHMWPE fiber in original white color and test by CTTC in 2014 and the tenacity was 31cN/dtex. Tested Item Result Standard Linear Density 1742.2dtex GB/T 19975-2005 Breaking Tenacity 31cN/dtex GB/T 19975-2005 CV of breaking tenacity 5.99% GB/T 19975-2005 Breaking elongation 3.20% GB/T 19975-2005 CV of breaking elongation 6.81% GB/T 19975-2005 Melting Point 140 degrees FZ/T 01057.6-2007 *The test results are transferred from below Chinese version. Part view of UHMWPE fiber test report – 1600D/960F

Read More »

Test report of 1600D UHMWPE Fiber in 2019

The test sample is 1600D/480F UHMWPE fiber in original white color and test by CTTC in 2019 and the tenacity was 32cN/dtex. Tested Item Result Standard Linear Density 1772.8dtex GB/T 19975-2005 Breaking Tenacity 32cN/dtex GB/T 19975-2005 CV of breaking tenacity 2.78% GB/T 19975-2005 Breaking elongation 3.36% GB/T 19975-2005 CV of breaking elongation 6.88% GB/T 19975-2005 Initial Modulus 1440cN/dtex GB/T 19975-2005 *The test results are transferred from below Chinese version. Part view of UHMWPE fiber test report – 1600D/480F

Read More »

Test report of 800D UHMWPE Fiber in 2021

The test sample is 800D UHMWPE fiber in original white color and test by DXLL in 2021 and the tenacity was 45.01cN/dtex. Tested Item Result Standard Linear Density 886dtex GB/T 14343-2008 Breaking Tenacity 45.01cN/dtex GB/T 19975-2005 CV of breaking tenacity 2.79% GB/T 19975-2005 Breaking elongation – GB/T 19975-2005 CV of breaking elongation – GB/T 19975-2005 Initial Modulus 1686cN/dtex GB/T 19975-2005 *The test results are transferred from below Chinese version. Part view of UHMWPE fiber test report – 800D

Read More »